A cast ring comes out of the mould looking like a ring and feeling like sandpaper. What happens next is the difference between a $40 ring and a $400 one.

Filing and emery

The sprue is cut, then the whole shank is filed true, then worked through four grades of emery paper. This is where a band becomes round and even.

Pre-polish, setting, final polish

We pre-polish before setting so the claws are never touched by a wheel, set the stone under a microscope, then polish the whole piece again on a separate wheel with no stone-contact.

Plating and the last check

Plated pieces go through an ultrasonic clean, a rhodium or gold bath, then a 24-hour humidity check before they are allowed into a box. Roughly one in forty fails that check and goes back to the bench.